Tim,
Way better than those who are niggardly with release agent.
John
gave us the "glue-in". Unless you are describing globbed on wax as a heavy coat, the film thickness of the release agent is in the microns thick range. If I want to come back out instead of being glued in I would always err on the heavy side.I thought less release agent was better... thinner gap between the metal and epoxy then. I know you can buff the crap out of Kiwi wax and it still works fine.
Don't the instructions say to let it cure for 24 hrs?
"instructions"....? What is the meaning of this foreign word you mention...?
At least that is my policy for most instructions. Too many instructions where written by the engineers that design the product. I would much rather help from someone that has actually done it before. I am still mad about the current state of automobiles. Ever try to change the spark plugs on 2006 Ford Expedition? What kind of engineer could come up with something like that...? ..........What was I talking about.....?
Tim