    Cool Explain

    What salts used how much processused bill b thanks

  2. #2
    Join Date
    Feb 2003
    Location
    Tennessee
    Posts
    5,159
    Bill - are you asking about annealing?

    Wilbur

  3. #3
    Join Date
    Dec 2003
    Location
    washington.........STATE that is.
    Posts
    10,106
    I use the old standard Oxynate #7 from the 40# pails....... I can't remember the mix because I just fire the burners up when I've a batch of bluing, but it's on the buckets

    I _think_ I use less than a bucket in a 5ft stainless steel tank????

    disremember

  4. #4
    Join Date
    Nov 2006
    Location
    Augusta, Maine & Palm Coast, Fl
    Posts
    5,992

    Very simple Bill

    Quote Originally Posted by bbrawand View Post
    What salts used how much processused bill b thanks
    A small Lee lead lead pot. A kit from the guy in Canada for about $100. Heat the salt to 750f or so and dip the cases in the molten salt for 5 or 6 seconds, toss them in water to dissolve any remaining salt, dry them ( I put mine in my kitchen oven @ 200 for a few minutes), let them cool and use them. Very easy. Be sure to get the case holder and the thermostat with thermocouple.

    Pete